They are actually a crystallization of amorphous silicon.

Prize winning photo at 50th photo contest hosted by the Japanese Society of Electron Microscopy in 1994.

Condition

  • Specimen: p-doped Si/SiO2/Si
  • Instrument: Transmission Electron Microscope H-9000NAR
  • Magnification : × 2,500
  • Accelerating voltage : 300 kV
*
All information related to these photographers is based on the information when the photo was taken.
*
This work was presented at the "photo contest" hosted by the Japanese Society of Microscopy.
*
Reproduction or republication without permission prohibited.
*