nanoart®

nano scale roller coaster

© Shuichi Takeuchi, Mine Nakagawa (Hitachi Science Systems, Ltd.)
© Mitsugu Sato, Atsushi Takane, Takeshi Ogashiwa (Hitachi High-Technologies corporation)
© Shouji Yoshida (Hitachi Research Laboratory, Hitachi, Ltd.)

At last, the amusement park of the nano scale was established.
This image is an example of observing the carbon nano-tube that the utilization to electron source of the flat displays panel and hydrogen storage elements of the fuel cell, etc., was observed by an in-lens FE-SEM. By using the focal depth expansion function, the aspect of the carbon nano-tubes with which intricately intertwine is observed clearly.
Someday in the near future, you might zoom out a visitor at this park.

At 58th photo contest hosted by the Japanese Society of Electron Microscopy in 2002.

Condition

  • Specimen: Carbon Nanotube
  • Instrument: Scanning Electron Microscope S-5200
  • Magnification: × 50,000
  • Accelerating voltage: 5 kV
*
All information related to these photographers is based on the information when the photo was taken.
*
This work was presented at the "photo contest" hosted by the Japanese Society of Microscopy.
*
Reproduction or republication without permission prohibited.
*
"nanoart" is registered trademark of Hitachi High-Technologies Corporation in Japan.