Skip to main content

Hitachi

Hitachi High-Tech GLOBAL

Find More Products

Company Profile

Company Name NGK ELECTRONICS DEVICES, INC.
Location Mi-ne, Yamaguchi, JAPAN
Established March, 1991
Capital 3,450 Million Yen
Net Sales
(FY ended 3/31/2020)
15,871 Million Yen
Number of Employees 520

Main Products

Ceramic Package

Recently data speed is further urged by digital coherent innovation. NGKED multilayer ceramic gives a solution with back-up of simulation technology.

Excellent electric characteristics (S-parameter)

In addition to transmission and receiver purpose, driver application package can be provided.

Ceramic FeedThrough

Ceramic FeedThrough is key part of Ceramic Package.

Pass band expansion beyond 55GHz

Line&Space = 75/75um Via diameter = 85um

RF Simulation Results for 64GB ICR

★ Simulated and measured results are very close!

Find More Products