Skip to main content

Hitachi

Hitachi High-Technologies GLOBAL

Let's look at the world of imagination !!
Real View Sample Observation Thermal Analysis System

In normal thermal analysis equipment, you can only determine what is happening based on the behavior of the DSC and TG curves; however, with the Real View Sample Observation Thermal Analysis System, you can view phenomena that cannot be understood by thermal analysis data alone.

The advantages of the Real View Thermal Analysis System

  1. Because the information you have obtained has increased, it now becomes easier to analyze data
  2. You can obtain the resulting knowledge from phenomena that you have not noticed until now
  3. It will be easier to analyze the causes of abnormal phenomena

Real View Thermal Analysis seen in videos

Introducing the Real View Thermal Analysis


STA7200RV+RV-3TG+AS-3T

  • * This option is not available for sell in Europe at the moment.


Functions of Real View® TA


STA7200RV+RV-2TG

Measurement Examples


Real View TG measurement of PET (41 seconds)


Real View TG measurement of NBR (52 seconds)


Real View TG measurement of wood (51 seconds)


Real View TG measurement of optical fiber (40 seconds)

DSC measurement of amorphous PET
(24 second)

DSC measurement of composite of HDPE and LDPE
(37 second)

DSC measurement of erasable ink
(27 second)

DSC measurement of optical fiber - 1
(28 second)

DSC measurement of optical fiber - 2
(30 second)

TG/DTA measurement of heat shrink material
(36 second)

DMA measurement of heat shrink material
(57 second)

Technical report (measurement example)

Technical report (measurement example)
TA No.24 Observing a sample during DSC measurement
TA No.73 You can see the sample change during measurement with the Sample Observation Unit
TA No.76 Observation of the Decomposition Behavior of PET by using Real View TG
TA No.77 Real View DSC of Pharmaceuticals, Salicin
TA No.78 Compatibility Observation of LDPE and HDPE using RV-DSC
Download Adobe Reader
In order to read a PDF file, you need to have Adobe® Reader® installed in your computer.