Hitachi

Real View TG measurement of NBR

The example shows the results from a rubber sample, first heated in nitrogen atmosphere and then in air atmosphere after cooling. In addition to quantitative determination of components by measuring weight losses, changes on sample profile such as color & shape and some events like flame spark from combustion are observed.