Skip to main content

Hitachi High-Tech
  1. Home
  2. Knowledge
  3. Analytical Systems
  4. Knowledge: Thermal Analysis
  5. Standards of Thermal Analysis

Standards of Thermal Analysis

List of standards supported with Hitachi’s thermal analysis and viscoelasticity.

ISO (International Organization for Standards)

ISO NO TITLE
ISO 11357-1 Plastics - Differential Scanning Calorimetry (DSC)
Part 1: General Principles
DSC
ISO 11357-2 Plastics - Differential Scanning Calorimetry (DSC)
Part 2: Determination of Glass Transition Temperature
DSC
ISO 11357-3 Plastics - Differential Scanning Calorimetry (DSC)
Part 3: Determination of Temperature and Enthalpy of Melting and Crystallization
DSC
ISO 11357-4 Plastics - Differential Scanning Calorimetry (DSC)
Part 4: Determination of specific heat capacity
DSC
ISO 11357-5 Plastics - Differential Scanning Calorimetry (DSC)
Part 5: Determination of Characteristic Reaction-curve Temperatures and Times, Enthalpy of Reaction and Degree of Conversion
DSC
ISO 11357-6 Plastics - Differential scanning calorimetry (DSC)
Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)
DSC
(OIT)
ISO 11357-7 Plastics - Differential Scanning Calorimetry (DSC)
Part 7: Determination of crystallization kinetics
DSC
ISO 11358-1 Plastics -- Thermogravimetry (TG) of polymers --
Part 1: General principles
TG
ISO 11358-2 Plastics -- Thermogravimetry (TG) of polymers
Part 2: Determination of activation energy
TG
ISO 11358-3 Plastics -- Thermogravimetry (TG) of polymers --
Part 3: Determination of the activation energy using the Ozawa-Friedman plot and analysis of the reaction kinetics
TG
ISO 11359-1 Plastics - Thermomechanical Analysis (TMA)
Part 1: General Principle
TMA
ISO 11359-2 Plastics - Thermomechanical Analysis (TMA)
Part 2: Determination of Coefficient of Linear Thermal Expansion and Glass Transition Temperature
TMA
ISO 11359-3 Plastics - Thermomechanical Analysis (TMA)
Part 3: Determination of penetration temperature
TMA
ISO 22768 Rubber, raw -- Determination of the glass transition temperature by differential scanning calorimetry (DSC) DSC
ISO 9924-1 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
TG
ISO 9924-2 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 2: Acrylonitrile-butadiene and halobutyl rubbers
TG
ISO 9924-3 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 3: Hydrocarbon rubbers, halogenated rubbers and polysiloxane rubbers after extraction
TG
ISO 6721-1 Plastics -- Determination of dynamic mechanical properties -- Part 1: General principles DMA
ISO 6721-4 Plastics -- Determination of dynamic mechanical properties -- Part 4: Tensile vibration -- Non-resonance method DMA
ISO 6721-5 Plastics -- Determination of dynamic mechanical properties -- Part 5: Flexural vibration -- Non-resonance method DMA
ISO 6721-6 Plastics -- Determination of dynamic mechanical properties -- Part 6: Shear vibration -- Non-resonance method DMA
ISO 6721-11 Plastics -- Determination of dynamic mechanical properties -- Part 11: Glass transition temperature DMA
ISO 6721-12 Plastics -- Determination of dynamic mechanical properties -- Part 12: Compressive vibration -- Non-resonance method DMA

ASTM (ASTM International)

ASTM NO TITLE
D3418-21 Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry DSC
D3895 - 19 Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry DSC
(OIT)
D4419-90(2021) Standard Test Method for Measurement of Transition Temperatures of Petroleum Waxes by Differential Scanning Calorimetry (DSC) DSC
D4591-22 Standard Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry DSC
D7028 - 07(2015) Standard Test Method for Glass Transition Temperature (DMA Tg) of Polymer Matrix Composites by Dynamic Mechanical Analysis (DMA) DMA
E793-06(2018) Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry DSC
E794-06(2018) Standard Test Method for Melting And Crystallization Temperatures By Thermal Analysis DSC, DTA
E928 - 19 Standard Test Method for Purity by Differential Scanning Calorimetry DSC
E967 - 18 Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers DSC, DTA
E968 - 02(2014) Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters DSC
E1131-20 Standard Test Method for Compositional Analysis by Thermogravimetry TG
E1269-11(2018) Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry DSC(Cp)
E1356-08(2014) Standard Test Method for Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry DSC
E1363-18 Standard Test Method for Temperature Calibration of Thermomechanical Analyzers TMA
E1545-22 Standard Test Method for Assignment of the Glass Transition Temperature by Thermomechanical Analysis TMA
E1640-18 Standard Test Method for Assignment of the Glass Transition Temperature By Dynamic Mechanical Analysis DMA
E1641-18 Standard Test Method for Decomposition Kinetics by Thermogravimetry Using the Ozawa/Flynn/Wall Method TG
E1824 - 19 Standard Test Method for Assignment of a Glass Transition Temperature Using Thermomechanical Analysis: Tension Method TMA
E1858-08(2015)e1 Standard Test Methods for Determining Oxidation Induction Time of Hydrocarbons by Differential Scanning Calorimetry DSC
E2040-19 Standard Test Method for Mass Scale Calibration of Thermogravimetric Analyzers TG
E2092 - 18a Standard Test Method for Distortion Temperature in Three-Point Bending by Thermomechanical Analysis TMA
E2113-18 Standard Test Method for Length Change Calibration of Thermomechanical Analyzers TMA
E2206-21 Standard Test Method for Force Calibration of Thermomechanical Analyzers TMA
E2254 - 18 Standard Test Method for Storage Modulus Calibration of Dynamic Mechanical Analyzers DMA
E2347-21 Standard Test Method for Indentation Softening Temperature by Thermomechanical Analysis TMA
E2550-21 Standard Test Method for Thermal Stability by Thermogravimetry TG
E2602-22 Standard Test Methods for Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry TM-DSC
E2716 - 09(2014) Standard Test Method for Determining Specific Heat Capacity by Sinusoidal Modulated Temperature Differential Scanning Calorimetry TM-DSC

JIS (Japan Industrial Standards)

JIS NO TITLE
JIS K 0129 General rules for thermal analysis
JIS K 7120 Testing methods of plastics by thermogravimetry TG
JIS K 7121 Testing methods for transition temperatures of plastics DSC
JIS K 7122 Testing methods for heat of transitions of plastics DSC
JIS K 7123 Testing methods for specific heat capacity of plastics DSC (Cp)
JIS K 7196 Testing method for softening temperature of thermoplastics film and sheeting by thermomechanical analysis TMA
JIS K 7197 Testing method for linear thermal expansion coefficient of plastics by thermomechanical analysis TMA
JIS K 6226-1 Rubber and rubber products
- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry
- Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
TG
JIS K 6226-2 Rubber and rubber products
- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry
- Part 2: Acrylonitrile-butadiene and halobutyl rubbers
TG
JIS H 7101 Method for determining the transformation temperature of shape memory alloys DSC
JIS R 3102 Testing method for average linear thermal expansion of glass TMA
JIS K 6240 Rubber, raw - Determination of the glass transition temperature by differential scanning calorimetry (DSC) DSC
JIS K 6394 Rubber, vulcanized or thermoplastic -- Determination of dynamic properties -- General guidance DMA
JIS K 6762 Double wall polyethylene pipes for water supply DTA/DSC
(OIT)
JIS K 4834 Measurement method of exothermic decomposition energy for explosive estimation DSC
JIS C 3660-410 Electric and optical fibre cables -- Test methods for non-metallic materials -- Part 410: Miscellaneous tests -- Test method for copper-catalyzed oxidative degradation of polyolefin insulated conductors DTA/DSC
(OIT)
JIS C 6481 Test methods of copper-clad laminates for printed wiring boards TMA
JIS G 5511 Low thermal expansive Fe-alloy castings TMA
JIS H 7151 Method of determining the crystallization temperatures of amorphous metals DSC, DTA
JIS H 7802 Testing method of ultrafine metal particles for ignition temperature by differential thermal analysis DTA
JIS R 1618 Measuring method of thermal expansion of fine ceramics by thermomechanical analysis TMA
JIS R 1672 Determination of specific heat of fiber-reinforced ceramics composite by differential scanning calorimetry methods DSC
(Cp)
JIS K 7095 Testing method for glass transition temperatures of carbon fibre reinforced plastics by thermal analysis DSC,TMA,DMA
JIS Z 2285 Measuring method of coefficient of linear thermal expansion of metallic materials TMA
JIS Z 3198-1 Test methods for lead-free solders
- Part 1: Methods for measuring of melting temperature ranges
DSC, DTA
JIS K 7244-1 Plastics - Determination of dynamic mechanical properties
- Part 1: General principles
DMA
JIS K 7244-4 Plastics - Determination of dynamic mechanical properties
- Part 4: Tensile vibration -- Non-resonance method
DMA
JIS K 7244-5 Plastics - Determination of dynamic mechanical properties
- Part 5: Flexural vibration -- Non-resonance method
DMA
JIS K 7244-6 Plastics - Determination of dynamic mechanical properties
- Part 6: Shear vibration -- Non-resonance method
DMA

IPC-TM-650 (Association Connecting Electronics Industries)

IPC NO TITLE
2.3.40 Thermal Stability TG
2.4.24 C Glass Transition Temperature and Z-Axis Thermal Expansion by TMA TMA
2.4.24.1 Time to Delamination (TMA Method) TMA
2.4.24.2 Glass Transition Temperature of Organic Films - DMA Method DMA
2.4.24.3 Glass Transition Temperature of Organic Films - TMA Method TMA
2.4.24.4 Glass Transition and Modulus of Materials Used in High Density Interconnection (HDI) and Microvias -DMA Method DMA
2.4.24.5 Glass Transition Temperature and Thermal Expansion of Materials Used In High Density Interconnection (HDI) and Microvias -TMA Method TMA
2.4.24.6 Decomposition Temperature (Td) of Laminate Material Using TGA TG
2.4.25 D Glass Transition Temperature and Cure Factor by DSC DSC
2.4.41 Coefficient of Linear Thermal Expansion of Electrical Insulating Materials TMA

Related products

With Standards-Based Guidance, users will be walked-through the processes to perform standards methods measurements according to organizations such as JIS, ISO, ASTM etc.

Products & Services