Medicine tablet (Foreign substances put on purposely)

Image of Medicine tablet (Foreign substances put on purposely)
Magnification : x600

Compositional contrast allows the determination of contaminants that may otherwise be difficult to find with a light microscope. Metal contaminants, etc. should be quickly identified by brighter BSE image compositional contrast. Oxford Energy Dispersive X-ray Spectrometer SwiftED3000 enables to conduct multipoint analysis by utilizing its intuitive operation. Furthermore EDX analysis can identify contaminants or root causes.

Spectrum 1

Image of Medicine tablet EDX spectrum1

Spectrum 2

Image of Medicine tablet EDX spectrum2

Spectrum 3

Image of Medicine tablet EDX spectrum3