Skip to main content

Hitachi

Hitachi High-Technologies in Korea

Real-time 3D analytical FIB-SEM NX9000

FIB-SEM System for True 3D Structural Analysis

The newly developed FIB-SEM system from Hitachi, the NX9000 incorporates an optimized layout for true high-resolution serial sectioning to tackle the latest demands in 3D structural analysis and for TEM and 3DAP analyses. The NX9000 FIB-SEM system allows the highest precision in material processing for a wide range of areas relating to advanced materials, electronic devices, biological tissues, and a multitude of other applications.

Features

  • The SEM column and FIB column are orthogonally arranged to optimize the column positioning for 3D structural analysis.
  • The combination of high-brightness cold-field-emission electron source and high-sensitivity optics support analysis of a wide range of materials from biological tissues to magnetic materials.
  • The Micro-sampling system and Triple Beam system allow high-quality sample preparation for TEM and atom-probe applications.

Ion milling and observation at normal incidence in real-time for true analytical imaging

The SEM column and FIB column are orthogonally arranged to realize normal incident SEM imaging of FIB cross sections.
Orthogonal column arrangement eliminates aspect deformation, foreshortening of cross-sectional images, and shift of the field of view (FOV) during serial section imaging, which cannot be avoided by conventional FIB-SEM systems. The NX9000 images enable highly accurate 3D structural analysis. Optical correlative microscopy can be applied easily due to the benefit of surface-planar EM imaging.

Conventional FIB-SEM , Orthogonally arranged FIB-SEM

Sample: Mouse brain neuron
Sample courtesy of Yoshiyuki Kubota, Ph.D., Neural Information Processing Systems (NIPS)

Cut & See·3D-EDS*1·3D-EBSD*1 available for a wide variety of materials

Cut&See

Cut & See supports high-resolution, high-contrast imaging of biological tissues, semiconductors, and magnetic materials, such as steel and nickel, at low accelerating voltages.
Serial section images can be collected with high throughput due to the proper geometry of the ion and electron column.

1nm step Cut&See , Serial section images

Sample: NAND flash memory
SEM accelerating voltage: 1 kV
Cutting interval: 1 nm
Number of cut: 300

3D-EDS*1

Serial section SEM images and serial section elemental maps can be collected using 3D-EDS.
The large-area silicon drift detector reduces the acquisition time and enables elemental mapping at low accelerating voltages.

3D-EDS

Sample: Fuel cell electrode
SEM accelerating voltage: 5 kV
Cutting interval: 100 nm
Number of cut: 212

Sample courtesy of Prof. Naoki Shikazono, University of Tokyo

3D-EBSD*1

Simultaneous SEM, FIB, and EBSD signals are obtained for 3D-EBSD without moving the stage during FIB sectioning and EBSD analysis. Accuracy and throughput of 3D crystal orientation analysis and segmentation yield high quality and less post-processing correction.

3D-EBSD

Sample: Ni
SEM accelerating voltage: 20 kV
Cutting interval: 150 nm
Number of cut: 150

*1:
Option

Hitachi patents:
US6118122, US6538254, US6828566, US7138628, US7345289, US7397050, US7397051, US7442942, US7525108, US7550750, US8198603, US8569719, US8642958, US8664598, and other patents, as of Jun., 2015

Specifications

Specifications
ItemsDescription
SEM Electron source Cold cathode field emission source
Accelerating voltage 0.1 - 30 kV
Resolution 2.1 nm@1 kV
1.6 nm@15 kV
FIB Ion source Ga liquid metal ion source
Accelerating voltage 0.5 - 30 kV
Resolution 4.0 nm@30 kV
Maximum probe current 100 nA
Standard detector In-column SED / In-column BSED / Chamber SED
Stage X 0 - 20 mm *2
Y 0 - 20 mm *2
Z 0 - 20 mm *2
θ 0 - 360° *2
τ -25 - 45° *2
Maximum sample size 6 mm x 6 mm, 2 mm thick
*2:
Stroke is limited by each sample holder

Application Data

Material Science

3D distribution analysis with multiple signals

Fuel cell electrode

Specimen: Fuel cell electrode SEM accelerating voltage: 0.3 kV
FOV: 20 µm
Cutting interval: 10 nm
Number of cut: 600

 

Semiconductor

3D structural analysis from serial section SEM images

Specimen: 3D NAND flash memory

 

High-precision site-specific lamella preparation

30 kV FIB

1 kV Ar

Specimen: 14 nm SoC device
Final milling: 1 kV Ar
Observation: HF-3300 Cold FE-TEM (Accelerating voltage: 300 kV)

 

Life science

3D reconstruction from serial section SEM images

Specimen: Mouse brain neuron

Article information on Hitachi technical magazine "SI NEWS"

Scientific Instrument NEWS SI NEWS

This journal addresses a wide range variety of research papers and useful application data using Hitachi science instruments. Those authors are notable researchers and Hitachi application engineers. This is an article of Real-time 3D analytical FIB-SEM NX9000

 

Applications(Global)

Hitachi FIB Application Data

Technical magazine
"SI NEWS"

This journal addresses a wide range variety of research papers and useful application data using Hitachi science instruments.

SCIENTIFIC INSTRUMENT NEWS

Tabletop Microscope (Benchtop SEM)| TM4000/TM3030Plus/TM3030 Dedicated Website

FE Electron Microscope IEEE Milestone Special Website