規格 – ISO/ASTM/JIS/IPC
弊社の熱分析・粘弾性装置が対応する各規格をご紹介しております。
ISO (International Organization for Standards)
| ISO NO | TITLE | タイトル | |
|---|---|---|---|
| ISO 11357-1 | Plastics - Differential Scanning Calorimetry (DSC) Part 1: General Principles |
プラスチック-示差走査熱量測定(DSC)- 第1部:通則 |
DSC |
| ISO 11357-2 | Plastics - Differential Scanning Calorimetry (DSC) Part 2: Determination of Glass Transition Temperature |
プラスチック-示差走査熱量測定(DSC)- 第2部:ガラス転移温度の測定 |
DSC |
| ISO 11357-3 | Plastics - Differential Scanning Calorimetry (DSC) Part 3: Determination of Temperature and Enthalpy of Melting and Crystallization |
プラスチック-示差走査熱量測定(DSC)- 第3部:融解及び結晶化の温度及び熱量の測定 |
DSC |
| ISO 11357-4 | Plastics - Differential Scanning Calorimetry (DSC) Part 4: Determination of specific heat capacity |
プラスチック-示差走査熱量測定(DSC)- 第4部:比熱容量の測定 |
DSC |
| ISO 11357-5 | Plastics - Differential Scanning Calorimetry (DSC) Part 5: Determination of Characteristic Reaction-curve Temperatures and Times, Enthalpy of Reaction and Degree of Conversion |
プラスチック-示差走査熱量測定(DSC)- 第5部:反応特性曲線温度及び時間,反応エンタルピー並びに変換の度合いの測定 |
DSC |
| ISO 11357-6 | Plastics - Differential scanning calorimetry (DSC) Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) |
プラスチック-示差走査熱量測定(DSC)- 第6部:酸化誘導時間(等温OIT)及び酸化誘導温度(動的OIT)の測定 |
DSC (OIT) |
| ISO 11357-7 | Plastics - Differential Scanning Calorimetry (DSC) Part 7: Determination of crystallization kinetics |
プラスチック-示差走査熱量測定(DSC)- 第7部:結晶化反応速度の測定 |
DSC |
| ISO 11358-1 | Plastics -- Thermogravimetry (TG) of polymers -- Part 1: General principles |
プラスチック-重合体の熱重量測定法(TG)- 第1部:通則 |
TG |
| ISO 11358-2 | Plastics -- Thermogravimetry (TG) of polymers Part 2: Determination of activation energy |
プラスチック-重合体の熱重量測定法(TG)- 第2部:活性化エネルギーの測定 |
TG |
| ISO 11358-3 | Plastics -- Thermogravimetry (TG) of polymers -- Part 3: Determination of the activation energy using the Ozawa-Friedman plot and analysis of the reaction kinetics |
プラスチック-重合体の熱重量測定法(TG)- 第3部:小沢-フリードマンプロットによる活性化エネルギーの測定及び反応速度の解析 |
TG |
| ISO 11359-1 | Plastics - Thermomechanical Analysis (TMA) Part 1: General Principle |
プラスチック-熱機械測定(TMA) 第1部:通則 |
TMA |
| ISO 11359-2 | Plastics - Thermomechanical Analysis (TMA) Part 2: Determination of Coefficient of Linear Thermal Expansion and Glass Transition Temperature |
プラスチック-熱機械測定(TMA) 第2部:線膨張係数及びガラス転移温度の測定 |
TMA |
| ISO 11359-3 | Plastics - Thermomechanical Analysis (TMA) Part 3: Determination of penetration temperature |
プラスチック-熱機械測定(TMA) 第3部:針入温度の測定 |
TMA |
| ISO 22768 | Rubber, raw -- Determination of the glass transition temperature by differential scanning calorimetry (DSC) | 生ゴム-示差走査熱量測定(DSC)によるガラス転移温度の測定 | DSC |
| ISO 9924-1 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers |
ゴム及びゴム製品-サーモグラビメトリーによる複合加硫物及び未加硫物の配合 第1部:ブタジエン,エチレン-プロピレンコポリマー及びターポリマー,イソブテン-イソプレン,イソプレン及びスチレン-ブタジエンゴム |
TG |
| ISO 9924-2 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 2: Acrylonitrile-butadiene and halobutyl rubbers |
ゴム及びゴム製品-サーモグラビメトリーによる複合加硫物及び未加硫物の配合 第2部:アクリロニトリル-ブタジエン及びハロブチルゴム |
TG |
| ISO 9924-3 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 3: Hydrocarbon rubbers, halogenated rubbers and polysiloxane rubbers after extraction |
ゴム及びゴム製品-サーモグラビメトリーによる複合加硫物及び未加硫物の配合 第3部:抽出後の炭化水素ゴム,ハロゲン化ゴム及びポリシロキサンゴム |
TG |
| ISO 6721-1 | Plastics -- Determination of dynamic mechanical properties -- Part 1: General principles | プラスチック-動的機械特性の測定方法 第1部:通則 |
DMA |
| ISO 6721-4 | Plastics -- Determination of dynamic mechanical properties -- Part 4: Tensile vibration -- Non-resonance method | プラスチック-動的機械特性の測定方法 第4部:引張振動-非共鳴法 |
DMA |
| ISO 6721-5 | Plastics -- Determination of dynamic mechanical properties -- Part 5: Flexural vibration -- Non-resonance method | プラスチック-動的機械特性の測定方法 第5部:曲げ振動-非共鳴法 |
DMA |
| ISO 6721-6 | Plastics -- Determination of dynamic mechanical properties -- Part 6: Shear vibration -- Non-resonance method | プラスチック-動的機械特性の測定方法 第6部:せん断振動-非共鳴法 |
DMA |
| ISO 6721-11 | Plastics -- Determination of dynamic mechanical properties -- Part 11: Glass transition temperature | プラスチック-動的機械特性の測定方法 第11部:ガラス転移温度 |
DMA |
| ISO 6721-12 | Plastics -- Determination of dynamic mechanical properties -- Part 12: Compressive vibration -- Non-resonance method | プラスチック-動的機械特性の測定方法 第12部:圧縮振動-非共振法 |
DMA |
ASTM (ASTM International)
| ASTM NO | TITLE | |
|---|---|---|
| D3418-21 | Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry | DSC |
| D3895 - 19 | Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry | DSC (OIT) |
| D4419-90(2021) | Standard Test Method for Measurement of Transition Temperatures of Petroleum Waxes by Differential Scanning Calorimetry (DSC) | DSC |
| D4591-22 | Standard Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry | DSC |
| D7028 - 07(2015) | Standard Test Method for Glass Transition Temperature (DMA Tg) of Polymer Matrix Composites by Dynamic Mechanical Analysis (DMA) | DMA |
| E793-06(2018) | Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry | DSC |
| E794-06(2018) | Standard Test Method for Melting And Crystallization Temperatures By Thermal Analysis | DSC, DTA |
| E928 - 19 | Standard Test Method for Purity by Differential Scanning Calorimetry | DSC |
| E967 - 18 | Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers | DSC, DTA |
| E968 - 02(2014) | Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters | DSC |
| E1131-20 | Standard Test Method for Compositional Analysis by Thermogravimetry | TG |
| E1269-11(2018) | Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry | DSC(Cp) |
| E1356-08(2014) | Standard Test Method for Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry | DSC |
| E1363-18 | Standard Test Method for Temperature Calibration of Thermomechanical Analyzers | TMA |
| E1545-22 | Standard Test Method for Assignment of the Glass Transition Temperature by Thermomechanical Analysis | TMA |
| E1640-18 | Standard Test Method for Assignment of the Glass Transition Temperature By Dynamic Mechanical Analysis | DMA |
| E1641-18 | Standard Test Method for Decomposition Kinetics by Thermogravimetry Using the Ozawa/Flynn/Wall Method | TG |
| E1824 - 19 | Standard Test Method for Assignment of a Glass Transition Temperature Using Thermomechanical Analysis: Tension Method | TMA |
| E1858-08(2015)e1 | Standard Test Methods for Determining Oxidation Induction Time of Hydrocarbons by Differential Scanning Calorimetry | DSC |
| E2040-19 | Standard Test Method for Mass Scale Calibration of Thermogravimetric Analyzers | TG |
| E2092 - 18a | Standard Test Method for Distortion Temperature in Three-Point Bending by Thermomechanical Analysis | TMA |
| E2113-18 | Standard Test Method for Length Change Calibration of Thermomechanical Analyzers | TMA |
| E2206-21 | Standard Test Method for Force Calibration of Thermomechanical Analyzers | TMA |
| E2254 - 18 | Standard Test Method for Storage Modulus Calibration of Dynamic Mechanical Analyzers | DMA |
| E2347-21 | Standard Test Method for Indentation Softening Temperature by Thermomechanical Analysis | TMA |
| E2550-21 | Standard Test Method for Thermal Stability by Thermogravimetry | TG |
| E2602-22 | Standard Test Methods for Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry | TM-DSC |
| E2716 - 09(2014) | Standard Test Method for Determining Specific Heat Capacity by Sinusoidal Modulated Temperature Differential Scanning Calorimetry | TM-DSC |
JIS (Japan Industrial Standards/日本規格協会)
| JIS NO | タイトル | TITLE | |
|---|---|---|---|
| JIS K 0129 | 熱分析通則 | General rules for thermal analysis | |
| JIS K 7120 | プラスチックの熱重量測定 | Testing methods of plastics by thermogravimetry | TG |
| JIS K 7121 | プラスチックの転移温度測定方法 | Testing methods for transition temperatures of plastics | DSC |
| JIS K 7122 | プラスチックの転移熱測定方法 | Testing methods for heat of transitions of plastics | DSC |
| JIS K 7123 | プラスチックの比熱容量測定方法 | Testing methods for specific heat capacity of plastics | DSC (Cp) |
| JIS K 7196 | 熱可塑性プラスチックフィルム及びシートの熱機械分析による軟化温度試験法 | Testing method for softening temperature of thermoplastics film and sheeting by thermomechanical analysis | TMA |
| JIS K 7197 | プラスチックの熱機械分析による線膨張率試験方法 | Testing method for linear thermal expansion coefficient of plastics by thermomechanical analysis | TMA |
| JIS K 6226-1 | ゴム - 熱重量測定による加硫ゴム及び未加硫ゴム組成分の定量 第1部:ブタジエンゴム,エチレンプロピレンゴム及びターポリマー,ブチルゴム,イソプレンゴム,スチレンブタジエンゴム |
Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers |
TG |
| JIS K 6226-2 | ゴム - 熱重量測定による加硫ゴム及び未加硫ゴム組成分の定量 第2部:アクリロニトリルブタジエンゴム(NBR,XNBR,HNBR)及びハロゲン化ブチルゴム |
Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 2: Acrylonitrile-butadiene and halobutyl rubbers |
TG |
| JIS H 7101 | 形状記憶合金の変態点測定方法 | Method for determining the transformation temperature of shape memory alloys | DSC |
| JIS R 3102 | ガラスの平均線膨張係数の試験方法 | Testing method for average linear thermal expansion of glass | TMA |
| JIS K 6240 | 原料ゴム-示差走査熱量測定(DSC)によるガラス転移温度の求め方 | Rubber, raw - Determination of the glass transition temperature by differential scanning calorimetry (DSC) | DSC |
| JIS K 6394 | 加硫ゴム及び熱可塑性ゴム ―動的性質の求め方― 一般指針 | Rubber, vulcanized or thermoplastic -- Determination of dynamic properties -- General guidance | DMA |
| JIS K 6762 | 水道用ポリエチレン二層管 | Double wall polyethylene pipes for water supply | DTA/DSC (OIT) |
| JIS K 4834 | 化学物質の爆発危険性評価手法としての発熱分解エネルギーの測定方法 | Measurement method of exothermic decomposition energy for explosive estimation | DSC |
| JIS C 3660-410 | 電気・光ファイバケーブル―非金属材料の試験方法― 第410部:各種試験―銅導体を被覆するポリオレフィン絶縁材料の銅触媒による酸化劣化試験 |
Electric and optical fibre cables -- Test methods for non-metallic materials -- Part 410: Miscellaneous tests -- Test method for copper-catalyzed oxidative degradation of polyolefin insulated conductors | DTA/DSC (OIT) |
| JIS C 6481 | プリント配線板用銅張積層板試験方法 | Test methods of copper-clad laminates for printed wiring boards | TMA |
| JIS G 5511 | 鉄系低熱膨張鋳造品 | Low thermal expansive Fe-alloy castings | TMA |
| JIS H 7151 | アモルファス金属の結晶化温度測定方法 | Method of determining the crystallization temperatures of amorphous metals | DSC, DTA |
| JIS H 7802 | 示差熱分析法による金属超微粒子の発火温度測定方法 | Testing method of ultrafine metal particles for ignition temperature by differential thermal analysis | DTA |
| JIS R 1618 | ファインセラミックスの熱機械分析による熱膨張の測定方法 | Measuring method of thermal expansion of fine ceramics by thermomechanical analysis | TMA |
| JIS R 1672 | 長繊維強化セラミックス複合材料の示差走査熱量法による比熱容量測定方法 | Determination of specific heat of fiber-reinforced ceramics composite by differential scanning calorimetry methods | DSC (Cp) |
| JIS K 7095 | 炭素繊維強化プラスチックの熱分析によるガラス転移温度測定法 | Testing method for glass transition temperatures of carbon fibre reinforced plastics by thermal analysis | DSC,TMA,DMA |
| JIS Z 2285 | 金属材料の線膨張係数の測定方法 | Measuring method of coefficient of linear thermal expansion of metallic materials | TMA |
| JIS Z 3198-1 | 鉛フリーはんだ試験方法 第1部:溶融温度範囲測定方法 |
Test methods for lead-free solders - Part 1: Methods for measuring of melting temperature ranges |
DSC, DTA |
| JIS K 7244-1 | プラスチック - 動的機械特性の試験方法 - 第1部: 通則 |
Plastics - Determination of dynamic mechanical properties - Part 1: General principles |
DMA |
| JIS K 7244-4 | プラスチック - 動的機械特性の試験方法 - 第4部: 引張り振動 - 非共振法 |
Plastics - Determination of dynamic mechanical properties - Part 4: Tensile vibration -- Non-resonance method |
DMA |
| JIS K 7244-5 | プラスチック - 動的機械特性の試験方法 - 第5部: 曲げ振動 - 非共振法 |
Plastics - Determination of dynamic mechanical properties - Part 5: Flexural vibration -- Non-resonance method |
DMA |
| JIS K 7244-6 | プラスチック - 動的機械特性の試験方法 - 第6部: せん断振動 - 非共振法 |
Plastics - Determination of dynamic mechanical properties - Part 6: Shear vibration -- Non-resonance method |
DMA |
IPC-TM-650 (Association Connecting Electronics Industries)
| IPC NO | TITLE | タイトル | |
|---|---|---|---|
| 2.3.40 | Thermal Stability | 熱安定性 | TG |
| 2.4.24 C | Glass Transition Temperature and Z-Axis Thermal Expansion by TMA | TMAによるガラス転移温度とZ軸の熱膨張率 | TMA |
| 2.4.24.1 | Time to Delamination (TMA Method) | 熱剥離試験 (TMA 法) | TMA |
| 2.4.24.2 | Glass Transition Temperature of Organic Films - DMA Method | 有機膜のガラス転移温度(DMA法) | DMA |
| 2.4.24.3 | Glass Transition Temperature of Organic Films - TMA Method | 有機膜のガラス転移温度(TMA法) | TMA |
| 2.4.24.4 | Glass Transition and Modulus of Materials Used in High Density Interconnection (HDI) and Microvias -DMA Method | 高密度インターコネクタ (HDI) とマイクロビアに使用される材料のガラス転移温度と弾性率(DMA法) | DMA |
| 2.4.24.5 | Glass Transition Temperature and Thermal Expansion of Materials Used In High Density Interconnection (HDI) and Microvias -TMA Method | 高密度インターコネクタ (HDI) とマイクロビアに使用される材料のガラス転移温度と熱膨張率(TMA法) | TMA |
| 2.4.24.6 | Decomposition Temperature (Td) of Laminate Material Using TGA | 熱重量分析(TGA)によるラミネート材の熱分解温度(Td) | TG |
| 2.4.25 D | Glass Transition Temperature and Cure Factor by DSC | 示差走査熱量測定(DSC)による、ガラス転移温度と硬化度 | DSC |
| 2.4.41 | Coefficient of Linear Thermal Expansion of Electrical Insulating Materials | 電気的絶縁回路の線膨張係数 | TMA |
関連製品
Software for NEXTAのガイダンス機能では、標準規格ガイダンスではJIS、ISO、ASTMなどの規格に沿った測定ができます。