Recently data speed is further urged by digital coherent innovation. NGKED multilayer ceramic gives a solution with back-up of simulation technology.
Excellent electric characteristics (S-parameter)
In addition to transmission and receiver purpose, driver application package can be provided.
Ceramic FeedThrough is key part of Ceramic Package.
Pass band expansion beyond 55GHz
Line&Space = 75/75um Via diameter = 85um
★ Simulated and measured results are very close!