Standards of Thermal Analysis
List of standards supported with Hitachi’s thermal analysis and viscoelasticity.
ISO (International Organization for Standards)
| ISO NO | TITLE | |
|---|---|---|
| ISO 11357-1 | Plastics - Differential Scanning Calorimetry (DSC) Part 1: General Principles |
DSC |
| ISO 11357-2 | Plastics - Differential Scanning Calorimetry (DSC) Part 2: Determination of Glass Transition Temperature |
DSC |
| ISO 11357-3 | Plastics - Differential Scanning Calorimetry (DSC) Part 3: Determination of Temperature and Enthalpy of Melting and Crystallization |
DSC |
| ISO 11357-4 | Plastics - Differential Scanning Calorimetry (DSC) Part 4: Determination of specific heat capacity |
DSC |
| ISO 11357-5 | Plastics - Differential Scanning Calorimetry (DSC) Part 5: Determination of Characteristic Reaction-curve Temperatures and Times, Enthalpy of Reaction and Degree of Conversion |
DSC |
| ISO 11357-6 | Plastics - Differential scanning calorimetry (DSC) Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) |
DSC (OIT) |
| ISO 11357-7 | Plastics - Differential Scanning Calorimetry (DSC) Part 7: Determination of crystallization kinetics |
DSC |
| ISO 11358-1 | Plastics -- Thermogravimetry (TG) of polymers -- Part 1: General principles |
TG |
| ISO 11358-2 | Plastics -- Thermogravimetry (TG) of polymers Part 2: Determination of activation energy |
TG |
| ISO 11358-3 | Plastics -- Thermogravimetry (TG) of polymers -- Part 3: Determination of the activation energy using the Ozawa-Friedman plot and analysis of the reaction kinetics |
TG |
| ISO 11359-1 | Plastics - Thermomechanical Analysis (TMA) Part 1: General Principle |
TMA |
| ISO 11359-2 | Plastics - Thermomechanical Analysis (TMA) Part 2: Determination of Coefficient of Linear Thermal Expansion and Glass Transition Temperature |
TMA |
| ISO 11359-3 | Plastics - Thermomechanical Analysis (TMA) Part 3: Determination of penetration temperature |
TMA |
| ISO 22768 | Rubber, raw -- Determination of the glass transition temperature by differential scanning calorimetry (DSC) | DSC |
| ISO 9924-1 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers |
TG |
| ISO 9924-2 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 2: Acrylonitrile-butadiene and halobutyl rubbers |
TG |
| ISO 9924-3 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 3: Hydrocarbon rubbers, halogenated rubbers and polysiloxane rubbers after extraction |
TG |
| ISO 6721-1 | Plastics -- Determination of dynamic mechanical properties -- Part 1: General principles | DMA |
| ISO 6721-4 | Plastics -- Determination of dynamic mechanical properties -- Part 4: Tensile vibration -- Non-resonance method | DMA |
| ISO 6721-5 | Plastics -- Determination of dynamic mechanical properties -- Part 5: Flexural vibration -- Non-resonance method | DMA |
| ISO 6721-6 | Plastics -- Determination of dynamic mechanical properties -- Part 6: Shear vibration -- Non-resonance method | DMA |
| ISO 6721-11 | Plastics -- Determination of dynamic mechanical properties -- Part 11: Glass transition temperature | DMA |
| ISO 6721-12 | Plastics -- Determination of dynamic mechanical properties -- Part 12: Compressive vibration -- Non-resonance method | DMA |
ASTM (ASTM International)
| ASTM NO | TITLE | |
|---|---|---|
| D3418-21 | Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry | DSC |
| D3895 - 19 | Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry | DSC (OIT) |
| D4419-90(2021) | Standard Test Method for Measurement of Transition Temperatures of Petroleum Waxes by Differential Scanning Calorimetry (DSC) | DSC |
| D4591-22 | Standard Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry | DSC |
| D7028 - 07(2015) | Standard Test Method for Glass Transition Temperature (DMA Tg) of Polymer Matrix Composites by Dynamic Mechanical Analysis (DMA) | DMA |
| E793-06(2018) | Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry | DSC |
| E794-06(2018) | Standard Test Method for Melting And Crystallization Temperatures By Thermal Analysis | DSC, DTA |
| E928 - 19 | Standard Test Method for Purity by Differential Scanning Calorimetry | DSC |
| E967 - 18 | Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers | DSC, DTA |
| E968 - 02(2014) | Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters | DSC |
| E1131-20 | Standard Test Method for Compositional Analysis by Thermogravimetry | TG |
| E1269-11(2018) | Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry | DSC(Cp) |
| E1356-08(2014) | Standard Test Method for Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry | DSC |
| E1363-18 | Standard Test Method for Temperature Calibration of Thermomechanical Analyzers | TMA |
| E1545-22 | Standard Test Method for Assignment of the Glass Transition Temperature by Thermomechanical Analysis | TMA |
| E1640-18 | Standard Test Method for Assignment of the Glass Transition Temperature By Dynamic Mechanical Analysis | DMA |
| E1641-18 | Standard Test Method for Decomposition Kinetics by Thermogravimetry Using the Ozawa/Flynn/Wall Method | TG |
| E1824 - 19 | Standard Test Method for Assignment of a Glass Transition Temperature Using Thermomechanical Analysis: Tension Method | TMA |
| E1858-08(2015)e1 | Standard Test Methods for Determining Oxidation Induction Time of Hydrocarbons by Differential Scanning Calorimetry | DSC |
| E2040-19 | Standard Test Method for Mass Scale Calibration of Thermogravimetric Analyzers | TG |
| E2092 - 18a | Standard Test Method for Distortion Temperature in Three-Point Bending by Thermomechanical Analysis | TMA |
| E2113-18 | Standard Test Method for Length Change Calibration of Thermomechanical Analyzers | TMA |
| E2206-21 | Standard Test Method for Force Calibration of Thermomechanical Analyzers | TMA |
| E2254 - 18 | Standard Test Method for Storage Modulus Calibration of Dynamic Mechanical Analyzers | DMA |
| E2347-21 | Standard Test Method for Indentation Softening Temperature by Thermomechanical Analysis | TMA |
| E2550-21 | Standard Test Method for Thermal Stability by Thermogravimetry | TG |
| E2602-22 | Standard Test Methods for Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry | TM-DSC |
| E2716 - 09(2014) | Standard Test Method for Determining Specific Heat Capacity by Sinusoidal Modulated Temperature Differential Scanning Calorimetry | TM-DSC |
JIS (Japan Industrial Standards)
| JIS NO | TITLE | |
|---|---|---|
| JIS K 0129 | General rules for thermal analysis | |
| JIS K 7120 | Testing methods of plastics by thermogravimetry | TG |
| JIS K 7121 | Testing methods for transition temperatures of plastics | DSC |
| JIS K 7122 | Testing methods for heat of transitions of plastics | DSC |
| JIS K 7123 | Testing methods for specific heat capacity of plastics | DSC (Cp) |
| JIS K 7196 | Testing method for softening temperature of thermoplastics film and sheeting by thermomechanical analysis | TMA |
| JIS K 7197 | Testing method for linear thermal expansion coefficient of plastics by thermomechanical analysis | TMA |
| JIS K 6226-1 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers |
TG |
| JIS K 6226-2 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 2: Acrylonitrile-butadiene and halobutyl rubbers |
TG |
| JIS H 7101 | Method for determining the transformation temperature of shape memory alloys | DSC |
| JIS R 3102 | Testing method for average linear thermal expansion of glass | TMA |
| JIS K 6240 | Rubber, raw - Determination of the glass transition temperature by differential scanning calorimetry (DSC) | DSC |
| JIS K 6394 | Rubber, vulcanized or thermoplastic -- Determination of dynamic properties -- General guidance | DMA |
| JIS K 6762 | Double wall polyethylene pipes for water supply | DTA/DSC (OIT) |
| JIS K 4834 | Measurement method of exothermic decomposition energy for explosive estimation | DSC |
| JIS C 3660-410 | Electric and optical fibre cables -- Test methods for non-metallic materials -- Part 410: Miscellaneous tests -- Test method for copper-catalyzed oxidative degradation of polyolefin insulated conductors | DTA/DSC (OIT) |
| JIS C 6481 | Test methods of copper-clad laminates for printed wiring boards | TMA |
| JIS G 5511 | Low thermal expansive Fe-alloy castings | TMA |
| JIS H 7151 | Method of determining the crystallization temperatures of amorphous metals | DSC, DTA |
| JIS H 7802 | Testing method of ultrafine metal particles for ignition temperature by differential thermal analysis | DTA |
| JIS R 1618 | Measuring method of thermal expansion of fine ceramics by thermomechanical analysis | TMA |
| JIS R 1672 | Determination of specific heat of fiber-reinforced ceramics composite by differential scanning calorimetry methods | DSC (Cp) |
| JIS K 7095 | Testing method for glass transition temperatures of carbon fibre reinforced plastics by thermal analysis | DSC,TMA,DMA |
| JIS Z 2285 | Measuring method of coefficient of linear thermal expansion of metallic materials | TMA |
| JIS Z 3198-1 | Test methods for lead-free solders - Part 1: Methods for measuring of melting temperature ranges |
DSC, DTA |
| JIS K 7244-1 | Plastics - Determination of dynamic mechanical properties - Part 1: General principles |
DMA |
| JIS K 7244-4 | Plastics - Determination of dynamic mechanical properties - Part 4: Tensile vibration -- Non-resonance method |
DMA |
| JIS K 7244-5 | Plastics - Determination of dynamic mechanical properties - Part 5: Flexural vibration -- Non-resonance method |
DMA |
| JIS K 7244-6 | Plastics - Determination of dynamic mechanical properties - Part 6: Shear vibration -- Non-resonance method |
DMA |
IPC-TM-650 (Association Connecting Electronics Industries)
| IPC NO | TITLE | |
|---|---|---|
| 2.3.40 | Thermal Stability | TG |
| 2.4.24 C | Glass Transition Temperature and Z-Axis Thermal Expansion by TMA | TMA |
| 2.4.24.1 | Time to Delamination (TMA Method) | TMA |
| 2.4.24.2 | Glass Transition Temperature of Organic Films - DMA Method | DMA |
| 2.4.24.3 | Glass Transition Temperature of Organic Films - TMA Method | TMA |
| 2.4.24.4 | Glass Transition and Modulus of Materials Used in High Density Interconnection (HDI) and Microvias -DMA Method | DMA |
| 2.4.24.5 | Glass Transition Temperature and Thermal Expansion of Materials Used In High Density Interconnection (HDI) and Microvias -TMA Method | TMA |
| 2.4.24.6 | Decomposition Temperature (Td) of Laminate Material Using TGA | TG |
| 2.4.25 D | Glass Transition Temperature and Cure Factor by DSC | DSC |
| 2.4.41 | Coefficient of Linear Thermal Expansion of Electrical Insulating Materials | TMA |
Related products
With Standards-Based Guidance, users will be walked-through the processes to perform standards methods measurements according to organizations such as JIS, ISO, ASTM etc.