List of standards related to thermal analysis and viscoelasticity.

ISO (International Organization for Standards)

No. Title
ISO 11357-1 Plastics - Differential Scanning Calorimetry (DSC)
Part 1: General Principles
ISO 11357-2 Plastics - Differential Scanning Calorimetry (DSC)
Part 2: Determination of Glass Transition Temperature
ISO 11357-3 Plastics - Differential Scanning Calorimetry (DSC)
Part 3: Determination of Temperature and Enthalpy of Melting and Crystallization
ISO 11357-4 Plastics - Differential Scanning Calorimetry (DSC)
Part 4: Determination of specific heat capacity
ISO 11357-5 Plastics - Differential Scanning Calorimetry (DSC)
Part 5: Determination of Characteristic Reaction-curve
Temperatures and Times, Enthalpy of Reaction and Degree of Conversion
ISO 11357-6 Plastics - Differential Scanning Calorimetry (DSC)
Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)
ISO 11357-7 Plastics - Differential Scanning Calorimetry (DSC)
Part 7: Determination of crystallization kinetics
ISO 11358 Plastics - Thermogravimetry (TG) of Polymers
General Principles
ISO 11358-2 Plastics - Thermogravimetry (TG) of Polymers
Part 2: Determination of activation energy
ISO 11359-1 Plastics - Thermomechanical Analysis (TMA)
Part 1: General Principle
ISO 11359-2 Plastics - Thermomechanical Analysis (TMA)
Part 2: Determination of Coefficient of Linear Thermal
Expansion and Glass Tansition Temperature
ISO 11359-3 Plastics - Thermomechanical Analysis (TMA)
Part 3: Determination of penetration temperature
ISO 11409 Plastics - Phenolic resins
Determination of heats and temperatures of reaction by differential scanning calorimetry
ISO 9924-1 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
ISO 9924-2 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 2: Acrylonitrile-butadiene and halobutyl rubbers
ISO 9924-3 Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry -
Part 3: Hydrocarbon rubbers, halogenated rubbers and polysiloxane rubbers after extraction
ISO 18373-1 Rigid PVC pipes - Differential scanning calorimetry (DSC) method -
Part 1: Measurement of the processing temperature
ISO 18373-2 Rigid PVC pipes - Differential scanning calorimetry (DSC) method -
Part 2: Measurement of the enthalpy of fusion of crystallites
ISO 21870 Rubber compounding ingredients - Carbon black -
Determination of high-temperature loss on heating by thermogravimetry
ISO 22768 Rubber, raw -- Determination of the glass transition temperature by differential scanning calorimetry (DSC)
ISO 6721-1 Determination of Dynamic Mechanical Properties
Part 1: General Principles
ISO 6721-4 Determination of Dynamic Mechanical Properties
Part 4: Tensile Vibration - Non-resonance Method
ISO 6721-5 Determination of Dynamic Mechanical Properties
Part 5: Flexural Vibration - Non-resonance Method
ISO 6721-6 Determination of Dynamic Mechanical Properties
Part 6: Shear vibration -- Non-resonance method
ISO 6721-12 Determination of Dynamic Mechanical Properties
Part 12: Compressive vibration -- Non-resonance method

JIS (Japan Industrial Standards)

No. Title
JIS K 0129 General rules for thermal analysis
JIS K 7120 Testing methods of plastics by thermogravimetry
JIS K 7121 Testing methods for transition temperatures of plastics
JIS K 7122 Testing methods for heat of transitions of plastics
JIS K 7123 Testing methods for specific heat capacity of plastics
JIS K 7196 Testing method for softening temperature of thermoplastics film and sheeting by thermomechanical analysis
JIS K 7197 Testing method for linear thermal expansion coefficient of plastics by thermomechanical analysis
JIS K 6226-1 Rubber and rubber products
- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry
-Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers
JIS K 6226-2 Rubber and rubber products
- Determination of the composition of vulcanizates and uncured compounds by thermogravimetry
- Part 2: Acrylonitrile-butadiene and halobutyl rubbers
JIS K 6762 Double wall polyethylene pipes for water supply
JIS C 6481 Test methods of copper-clad laminates for printed wiring boards
JIS G 5511 Low thermal expansive Fe-alloy castings
JIS H 7101 Method for determining the transformation temperature of shape memory alloys
JIS H 7151 Method of determining the crystallization temperatures of amorphous metals
JIS R 1618 Measuring method of thermal expansion of fine ceramics by thermomechanical analysis
JIS R 3102 Testing method for average linear thermal expansion of glass
JIS Z 2285 Measuring method of coefficient of linear thermal expansion of metallic materials
JIS Z 3198-1 Test methods for lead-free solders - Part 1: Methods for measuring of melting temperature ranges
JIS K 7244-1 Plastics - Determination of dynamic mechanical properties
- Part 1: General principles
JIS K 7244-4 Plastics - Determination of dynamic mechanical properties
- Part 4: Tensile vibration -- Non-resonance method
JIS K 7244-5 Plastics - Determination of dynamic mechanical properties
- Part 5: Flexural vibration -- Non-resonance method
JIS K 7244-6 Plastics - Determination of dynamic mechanical properties
- Part 1: General principles