The newly incorporated balance control technology ensures the microgram-level baseline stability and reproducibility on top of our highly acclaimed horizontal digital dual beam balance system. The NEXTA STA series has following features;
High temperature control technology that handles a variety of temperature programs
Available DSC measurement, it makes specific heat capacity measurements available
The sample observation and measurement, Hitachi’s pioneering key feature
Includes the newly designed flow channels for high-level gas exchange

In addition to conventional applications, the NEXTA STA series shows its strength in analyses such as quantitative determination of the constituents of advanced materials, composite materials, and trace amounts of moisture.

Features

1. World class baseline performance

The NEXTA STA series incorporates a new balance control technology in addition to the horizontal digital dual beam system that has been well received in our previous models. Conventionally, baseline drift occurs due to hysteresis in the temperature program or surrounding environmental factors. However, by incorporating a new balance technology, the NEXTA STA series achieved baseline stability that is not affected by the temperature program.

Digital horizontal differential system

2. Broad measurement application using high temperature control technology

The NEXTA STA series heating furnace has the improved temperature control technology which realizes several temperature programs, such as heating at a constant heating rate, repetition heating and cooling, heating up and hold isothermal, temperature modulated DSC, and controlled reaction rate thermal analysis.

-

3. Available DSC measurement on the NEXTA STA series - Specific heat capacity measurement over the wide temperature range achieved by DSC

The NEXTA STA series showcases an evolution from DTA to DSC, enabling simultaneous thermogravimetry and DSC measurement, which defines it from its predecessors. In addition, by using temperature modulated DSC, specific heat capacity measurements are achieved over a wide temperature range that cannot be measured by (the) standalone DSC.

-
-

4. “Real View®” Sample Observation Option

The well-received “Real View®” option has been further developed.
Not only are samples observed while measurements are in progress, but various analysis features have been incorporated, such as digital zoom, image analysis, length measurement capability, and color analysis, which can support a variety of applications.

-

* “Real View” is a registered trademark of Hitachi High-Tech Analysis Corporation in the U.S, Brazil, China, India, Turkey, the European Union, and Japan.

Specifications

  STA200 STA200RV STA300
Balance Type Horizontal Differential Type
Temperature Range Ambient to 1,100°C Ambient to 1,000°C Ambient to 1,500°C
TG Baseline drift 1) <10 ug
TG Baseline Stability 2) <10 ug
DSC Function Standardly equipped
Specific Heat Capacity Measurement Available (Optional)
Temperature Precision +/-0.07°C
Temperature Accuracy +/-0.2°C
Real View®  N/A Optional N/A
Gas Control Integrated Mass Flow controller

1) Amount of Baseline drift at heating up to 1000°C with 20°C/min

2) Amount of baseline drift at 1000°C hold in 60min

Video

Citations

Applications of thermal analysis and viscoelastic equipment.

Describing the principles of thermal analysis and viscoelastic equipment.

Understand how your samples will perform with Hitachi thermal analyzers.

Thermal analysis software that features a guidance function and a new measurement mode that is very easy to use, even for beginners.

On-Demand Webinars for Thermal Analysis.

Standards of thermal analysis and viscoelastic equipment.

References and presentation documents regarding thermal analysis and viscoelasticity.

The trademark that represents our strong bond with the customer and shows our pledge to connect science and society to create new value.

Timeline of HITACHI Thermal Analysis Products.

Related Links

Brochure

Contact Us