Kozue
The structure looks like treetop is an aggregate of colloidal gold particles. The structure was formed by an electron beam irradiation in a transmission electron microscope.
At 56th photo contest hosted by the Japanese Society of Electron Microscopy in 2000.
Condition
Specimen : Colloidal gold particle on a carbon film
Instrument : Cold Field Emission Transmission Electron Microscope HF-2000
Magnification : × 2,000
*All information related to these photographers is based on the information when the photo was taken.