The small bouquet was found in the electron microscope. This is a SEM image of synthesized zeolite used for a catalyst in a variety of industrial applications. The structure of petal increases surface area and improves performance of catalyzer.

At 65th photo contest hosted by the Japanese Society of Microscopy in 2009.

Condition

  • Specimen: Synthesized zeolite
  • Instrument: Ultra-high Resolution Scanning Electron Microscope SU8000
  • Accelerating voltage: 2kV
*
All information related to these photographers is based on the information when the photo was taken.
*
This work was presented at the "photo contest" hosted by the Japanese Society of Microscopy.
*
Reproduction or republication without permission prohibited.
*
"nanoart" is registered trademark of Hitachi High-Tech Corporation in Japan.